Acrylic letter cutting

Acrylic letter nest with chip-break bits before a Friday install.

Clear acrylic letter cutouts lie on a wooden sheet in a CNC workshop with router bits and spindle holders nearby.

The sign shop’s urgent acrylic letter run

Careful tool selection and feed adjustments gave crisp edges and zero melting, setting a new shop standard.

Related: workshop guides and the tool range.

On a busy week, a Midrand sign shop took on a multi-layer acrylic letter job for a major shopping centre. The team faced a hard deadline for Friday morning handover, with sheets lined up for nested routing. Their old solid-carbide spirals had left burring and some heat haze last project, so this time they needed a cleaner, faster cut that would avoid wrestling with stubborn film and polishing edges.

The CNC router was in a compact workshop, running on vacuum hold-down with a standard MDF spoilboard. Humidity was moderate as winter settled in, but the shop still struggled with acrylic swarf sticking in tight corners, especially on smaller radius letters.

  • Job required tight tolerances
  • Previous bits left burrs and melting
  • Vacuum table with MDF spoilboard
  • Acrylic swarf clung to sharp inside curves

Chip-breaker spiral bits and feeds dialled for clean acrylic edges

Our Sunnyrock team suggested switching to our 6 mm and 8 mm up-cut acrylic chip-breaker spirals for the main nests, plus a 4 mm single-flute for small inner details. We advised their team or a qualified contractor to fit fresh ER32 collets, check runout under 0.01 mm with a dial indicator, and keep stick-out below 28 mm for rigidity. These chip-breaker bits disrupted the long acrylic chip, breaking it into smaller curls so it could clear out quickly with air blast.

We recommended starting at 2.5 to 4 metres per minute feed, 16 000 to 18 000 rpm, and a depth-of-cut at half the diameter. Stepdown and stepover were set conservatively on the first sheets, then increased after test passes showed zero melting or re-weld. The shop used air instead of mist cooling and kept the dust-extractor running for every sheet. Toolpaths were reprogrammed to ramp in on tabs, minimising plunge marks.

  • Up-cut chip-breaker spirals for main passes
  • Single-flute for tight radii
  • Runout checked and collet cleaned
  • Air blast cleared swarf, no mist needed
  • Ramp-in moves used for tab entry

Setting a new workshop standard and lessons for next time

After the rush, the shop started using chip-breaker bits for all their acrylic jobs, keeping edge finishing to a minimum. They now clean their collets and holders weekly, and keep an eye on spindle runout with each bit change. Printable speed and tool-life cards from CuTool are pinned up above the controller.

Next time, we would have pre-checked their vacuum hold-down for leaks before the rush. We’d also offer an AlTiN-coated bit for any routed components in ACM or foamed PVC, since the same feed strategies are not always ideal across those materials. If the shop moves to thicker acrylic or foam, we’ll recommend a compression spiral for top and bottom edge quality.

  • Chip-breaker bits now standard on acrylic
  • Regular collet cleaning routine started
  • Tool-life cards visible at controller
  • Future jobs may trial compression cutters for thicker stacks

What our Cutting Tool customers say

Verified Google reviews

Tell us about the job you need to cut

Send a note through our contact form with your machine, spindle and collet size, the material and thickness, the finish you need and your area, and we will come back with practical cutter options and a quote.

Open the contact form